You are here: English gizmag Atomic layer deposition and art conservancy – a marriage made in Maryland

Atomic layer deposition and art conservancy – a marriage made in Maryland

User Rating: / 0
PoorBest 

Antoine Louis Barye's 1865 Walking Lion is a perfect candidate for preservation via atomic...

Silver is a remarkable medium for artistic expression. It takes well to engraving, sculpting, casting, and fine detail while also having sufficient strength (especially in alloys) to insure the durability of art objects formed from this metal. Unfortunately, silver tarnishes when exposed to moist air, and removing layers of tarnish can damage the fine detail of artistic treasures. A new method for preventing the ravages of silver tarnish is now being developed by researchers in Maryland. .. Continue Reading Atomic layer deposition and art conservancy – a marriage made in Maryland

Section: Science

Tags: , , , ,

Related Articles:

Read all
Comment Policy:
We pre-moderate any comments and welcome all kinds of thoughts, supportive, dissenting, critical or otherwise. We delete or censor comments that are:

* abusive
* off-topic
* contain personal attacks, or against any company or organization
* promote hate of any kind
* use excessively foul language
* is blatantly spam or advertising

We do not discriminate based on the person who is posting, and we never censor comments for political or ideological reasons. We never delete an appropriate comment because we disagree with its viewpoint or ideology, and we never publish an inappropriate comment because we agree with or support its viewpoint or ideology.


Attention spammers: we manually approve all comments. Spamming and blatant advertising will NOT be published on this site and is deleted immediately, you've been warned, do not waste your time here.

Add comment

Security code
Refresh